Polyimide curing process.
2006-06-07
Lung-hao Hu
Polyimide curing process.
Lung-hao Hu
2006-06-07
I met a problem with polyimide based humidity sensors
I used polyimide to be a dielectric layer.
The bottom electrode is gold pattern and the top electrode is either copper or
gold.
I used thermal evaporator to coat with copper layer and the sensors work very
well after the polyimide absorpt the moisture.(i.e, I can see the huge
capacitance change).
But I used e-beam evaporator to coat with gold; and every sensor is
shorted.(i.e, there is a resistance between these two electrodes)
The curing process of polyimide is that heat it at 150C for 30 min and increase
the temp. to 350C for 30 min.
Should it be fully cured?? but I skip one step that is to cure and ramp to 350C
in inert gas.
Is it possible the ion-beam attacking the polyimide or is there some problem due
to the curing process ??
Is there someone who can tell me the reason why e-beam evaporation doesn't work
and make my sensors short.
Any possible reason is welcomed.

Lung-hao Hu

Graduate Student

Dept.of Mechanical Engineering
Univ.of Colorado Boulder
UCB 427 CO 80309 U.S.A
Email:[email protected]
Tel:303-786-1702(H)
    303-492-6107(O)
Fax:303-492-3498
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics