MEMSnet Home: MEMS-Talk: swell- or shrinkable material
swell- or shrinkable material
2006-06-16
Harald Walter
2006-06-16
[email protected]
swell- or shrinkable material
[email protected]
2006-06-16
How much shrink or swell, 1-3% or 50 to 70%.

Need to be more specific as to the temperature range.

You are asking to design a polymer to a specific Tg (glass transisition) and
softening point.

Rob