MEMSnet Home: MEMS-Talk: Permalloy electroplating solution
Permalloy electroplating solution
2006-06-30
Bin Wang
2006-07-11
IGOR KADIJA
2006-07-01
Bill Moffat
Permalloy electroplating solution
Bill Moffat
2006-07-01
I do not think you can electroplate alloys only pure metals.  Bill Moffat

________________________________

From: [email protected] on behalf of Bin Wang
Sent: Fri 6/30/2006 3:52 PM
To: [email protected]
Subject: [mems-talk] Permalloy electroplating solution

Hi all,

I want to electroplate permalloy on gold seed layer. Could anyone
recommend a vendor of the bath solution for permalloy
electroplating? Thanks.

Bin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
The Branford Group