A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: Nickel adhesion with gold seed laye
RE: Nickel adhesion with gold seed laye
2006-07-02
Behraad Bahreyni
photolithography: Front-To-Back Alignment
2006-07-02
Andrea Mazzolari
2006-07-04
walter essinger
2006-07-05
Jim Beall
RE: Nickel adhesion with gold seed laye
Behraad Bahreyni
2006-07-02
Hi,

   I do not think that the stress is the only problem. You might need
another layer of metal to improve the adhesion between the gold and
Nickel layers or use a metal like copper, if possible, for your seed
layer. It makes sense that the bottom surface of the Ni layer is smooth
because it is grown on top of the gold layer. However, as the Ni film
grows thicker it becomes rougher (you can reduce the roughness by
modifying the DC plating current (which is common for Ni plating) or by
pulse electroplating.

   Good luck,
   Behraad


>
> Subject:
> [mems-talk] Nickel adhesion with gold seed layer
> From: "g.balsubra manian" 
> Date: Fri, 30 Jun 2006 09:42:25 -0700 (PDT)
> To: [email protected]
> To: [email protected]
>
> Guys.,
>
> I electroplated Ni on Gold/Cr/Si (gold is seed layer).
> But after few hrs.,Nickel adhesion is lost and gets
> peeled off. I suppose this is due to the stress
> initiated during Ni electrodeposition.
>
> When viewing under microscope, The top surface of
> Peeled Ni is rough., Bottom surface is very smooth.
>
> Whether increasing the roughness of seed layer either
> by plasma oxidation technique will help???.
>
> Thanks
>
> Bala.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics