MEMSnet Home: MEMS-Talk: How to remove the PMMA etching residue.
How to remove the PMMA etching residue.
2006-08-15
Xiaojing Zou
2006-08-16
Scott McWilliams
2006-08-16
Xiaojing Zou
2006-08-16
Scott McWilliams
2006-08-16
Xiaojing Zou
2006-08-16
乔大勇
How to remove the PMMA etching residue.
Xiaojing Zou
2006-08-15
Hi:

    I did some CF4 and CHF3 etching SiO2 using PMMA as mask. But I found that
there is alway something left around the etched SiO2.  Does anybody have these
kinda experience about removal of these stuff ?? (It cannot be removed by
acetone)


Best Regards

Xiaojing Zou
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering
Nano-Master, Inc.