Wet etching of Quartz wafer
2006-09-09
Lin Yu
2006-09-12
Jesse D Fowler
2006-09-12
Jesse D Fowler
Wet etching of Quartz wafer
Jesse D Fowler
2006-09-12
Excuse me, I made a mistake. It's actually  Dr. Hiroshi Toshiyoshi.

Jesse Fowler

>From Jesse D Fowler 
Sent by: [email protected] 09/11/2006 17:10
To General MEMS discussion 
Subject Re: [mems-talk] Wet etching of Quartz wafer


Hello Lin,

If it's just fused quartz, it should be etching WAY faster than it is.
Something's coating it, or something's wrong with you HF.

If you're trying to etch single-crystal quartz, a little heat will go a
long way. Dr. Hiroshi Yoshi wrote a paper about etching single-crystal
quartz about 6 years ago. If I remember correctly, he was using BOE heated
in a boiling water bath.

Be careful with this stuff. I inquired with my lab manager about doing
this with concentrated HF, and he told me no way without a teflon coated
reflux ($5000 at the time).
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation