MEMSnet Home: MEMS-Talk: evaporation deposition
evaporation deposition
2006-09-25
Rupesh Sawant
2006-09-25
Karthik Sriram Lakshmi Narasimhan
2006-09-25
J.J wang
2006-09-25
prabhu arumugam
2006-09-27
[email protected]
evaporation deposition
prabhu arumugam
2006-09-25
hello Rupesh,
Pirana clean your wafers.

--- "J.J wang"  wrote:

> 1) Clean your glass wafer thouroughly.
> 2) Try a little bit thicker chrome
> 3) DON'T use ultrasonic
>