MEMSnet Home: MEMS-Talk: Polymerisation of PDMS
Polymerisation of PDMS
2006-10-03
RABBIA Laurent
2006-10-03
Gareth Jenkins
2006-10-03
Matthew Davies
2006-10-03
Barbara Cortese
Polymerisation of PDMS
Matthew Davies
2006-10-03
60 deg C and 4 hours are the standard conditions I use.

Matt

University of Hertfordshire

-----Original Message-----
From: RABBIA Laurent [mailto:[email protected]]
Sent: Tuesday, 3 October 2006 8:26 AM
To: '[email protected]'
Subject: [mems-talk] Polymerisation of PDMS

Hello everybody,

Please, someone can tell me which is the  temperature and time for complete
polymerisation of PDMS ? I know there is many process on it but in your
opinion which is the best ?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group