A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Partial Metallization of Vertical Walls
Partial Metallization of Vertical Walls
2006-10-14
Huaibin Zhang
Partial Metallization of Vertical Walls
2006-10-16
Xiaoguang "Leo" Liu
2006-10-16
g.balsubra manian
Nickel evaporation on PMMA!!!
2006-10-23
madhav rao
2006-10-23
Michael Rust
Nickel evaporation
2006-10-25
madhav rao
2006-10-26
Brent Garber
Partial Metallization of Vertical Walls
Huaibin Zhang
2006-10-14
---- Original message ----
>Date: Fri, 13 Oct 2006 19:31:48 -0400
>From: "Xiaoguang \"Leo\" Liu" 
>Subject: [mems-talk] Partial Metallization of Vertical Walls
>To: "General MEMS discussion" 
>
>Dear all
>I've been working on a project in fabricating cavity electromagnetic
>resonators that require partial metallization of the side walls. For
>example, I would like to produce a rectangular cavity  in the silicon
>substrate by DRIE. I would then want 2 of the 4 side walls to be
>metallized with gold while keeping the other 2 silicon. I've thought
>really hard about this but could not find a way to meet the
>requirement. The cavity in consideration is about 1mmx1mm big.
>
>Does anybody have good suggestions? Thanks a lot

Wow, it is a challenging task. Good thing is that 1mm x 1mm is not too hard to
handle. I have few questions want to know: (1) how many cavities do you need to
make?
(2) What is the relative position of the two side walls? Do they have to be in
the opposite side?

Huaibin

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Harrick Plasma, Inc.