A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: temporary bonding solutions
temporary bonding solutions
2006-11-05
Sebastian Sosin
2006-11-06
Mathieu Foquet
2006-11-06
ssood
2006-11-07
Barrie VanDevender
2006-11-07
Brubaker Chad
temporary bonding solutions
Barrie VanDevender
2006-11-07
This should work fine for 250um thick material.


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Mathieu Foquet
Sent: Monday, November 06, 2006 12:28 PM
To: Sebastian Sosin; [email protected]
Subject: RE: [mems-talk] temporary bonding solutions

Revalpha thermal release tape is one idea. (Nitto Denko)

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Sebastian Sosin
Sent: Sunday, November 05, 2006 7:54 AM
To: [email protected]
Subject: [mems-talk] temporary bonding solutions

I am looking for a temporary bonding solution that can be removed
without solvents (heat, UV.). It may be glue or adhesive tape. Does
anyone know any products like this?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group