MEMSnet Home: MEMS-Talk: about double coating and lithography of thick SPR220
about double coating and lithography of thick SPR220
2006-11-08
Zhang Xiao Qiang
Glass to glass bonding
2006-11-08
Hyun Chul Jung
2006-11-08
sokwon Paik
2006-11-08
Joseph Grogan
2006-11-09
邵建波
2006-11-09
Gareth Jenkins
2006-11-09
Y-bean Zhang
2006-11-09
Rashid, Mamun
2006-11-09
Indu Shekhar Bajpayee
2006-11-10
Anil Agiral
2006-11-10
Zhang Xiao Qiang
about double coating and lithography of thick SPR220
Zhang Xiao Qiang
2006-11-08
Dear friends

Anyone has the experiences about double/multi coating and lithography of
thick SPR220. I would like to use it get a near vertical side wall of my
patterns: the holes with aspect ratio of 2:1 and diameter of 2-6 micron.
I believe it is better than AZP 4620 as their datasheet show.

Any comments and recommendation are welcomed and highly appreciated.

Thank you & have a nice day!
Best regards!

Dr. Zhang XiaoQiang
Singapore-MIT Alliance
Department of Materials Science and Engineering
National University of Singapore
Email:[email protected]
Tel: +65-6516 1266
Fax: +65-6874 2081
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.