MEMSnet Home: MEMS-Talk: Silicon nitride residual stress
Higher electrical resistivity of electroplated copper ?
2006-11-25
Pradeep Dixit
Higher electrical resistivity of electroplated copper ?
2006-11-27
Kagan Topalli
Silicon nitride residual stress
2006-11-27
Andrea Mazzolari
2006-11-28
Darius
Higher electrical resistivity of electroplated copper ?
2006-11-27
David Nemeth
Silicon nitride residual stress
Darius
2006-11-28
Andrea,

Yes, micromaschined cantilever or bridge deformation is often used as a thin
films intrinsic stress measurement tool. I consider you to read these
papers:

J. Micromech. Microeng. 15 (2005) 608-614
Smart Mater. Struct. 15 (2006) S29-S38
J. Micromech. Microeng. 13 (2003) 686-692

Good luck

Darius


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Andrea Mazzolari
Sent: Monday, November 27, 2006 9:48 PM
To: 'General MEMS discussion'
Subject: [mems-talk] Silicon nitride residual stress


Hi all.
I need to determine residual stress in LPCVD silicon nitride.
Realizing silicon nitride cantilevers whould be possibile to measure silicon
nitride residual stress.
Measuring not-loaded cantilever deflection it whould be possible to
determine stress gradient, is this correct?
Whould be possible to measure also residual stress starting from silicon
nitride cantilevers ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
Mentor Graphics Corporation