purge with N2
2007-01-03
abdelyamine
2007-01-03
Michael D Martin
2007-01-04
Qiao Dayong
purge with N2
abdelyamine
2007-01-03
Hello

I've found on flow diagram of my equipment (Spray Acid Tool), that the tanks
of chemicals (H2SO4, HF.) are purged with N2. Could anyone tell me why,
please!!