MEMSnet Home: MEMS-Talk: Re: Why oxidation rate of polysilicon is much higher than that of single-crystal silicon(100)
Re: Why oxidation rate of polysilicon is much higher than that of single-crystal silicon(100)
2007-01-25
Michael Larsson
2007-01-26
PRAMOD GUPTA
Re: Why oxidation rate of polysilicon is much higher than that of single-crystal silicon(100)
Michael Larsson
2007-01-25
Hi Jay,

At a guess, I would say this is predominantly due to the presence of
grain boundaries. These are regions of high(er) energy, compared to
the rest of the xtal structure, meaning GBs are more active/reactive,
and more prone to oxidation (along with other chemical reactions with
Si). O2 diffusion rates are probably also higher along GBs, due to the
disorder in the regular xtal lattice, promoting more rapid oxidation.
I would say that increased diffusion rates at GBs are the main reason
for the increased oxidation rates

Following the thermodynamic argument: GBs introduce disorder to the
xtal structure, increasing its energetic state.  Thermodynamics shows
that all things in nature tend towards a state of lower energy, thus
the poly-Si will strive to do this at any opportunity (and more so
than SC Si). Oxidation is a mechanism by which the energy state of
many systems are reduced (e.g. rust in metals).

Regards,

Michael


> From: wanhong Cheung 
> To: [email protected]
> Date: Wed, 24 Jan 2007 08:45:43 -0800 (PST)
> Subject: [mems-talk] Why oxidation rate of polysilicon is much higher than
that of single-crystal silicon(100)
> Dear Members,
>
>  Can any one tell me why oxidation rate of polysilicon is much higher than
that of single-crystal silicon(100)
>
> Thanks
>
> Jay
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review