Nik Dee
2007-02-03
Hi guys, I am currently using a Copper plating solution (Water, Copper Sulphate,
Sulphuric Acid, NaCl and CUbath copper brightener) on gold seed layer. I try to
keep the plating rate to 30mA / cm2. I have noticed sometimes that the copper
plated on the seed surface is not bright enough and it gets a pink colour. Do
you have any idea what the reason for that might be?

Nik Dee


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics
Addison Engineering