silver electroplating
2007-01-31
Rupesh Sawant
2007-02-21
g.balsubra manian
silver electroplating
g.balsubra manian
2007-02-21
Rupesh.,

4o gm silver chloride
2oo gm potassium ferrocyanide
20 gm potassium carbonate
stainless steel or silver anodes
6o-8o C temp.,1o-15 A/sq.ft.

Here is the non-cyanide silver bath.

Bala.


--- Rupesh Sawant  wrote:

> hi,
> I am trying to electroplate a silver on a glass
> slide. I am using
> Ammoniacal SIlver Solution (0.72mol/L of NH3 (150ml)
> + 0.93gm of
> Silver nitrate crystals). THe electroplating is
> carried out at 0.1 A
> and 1.74 V. But the silver which is plated on my
> slide is not uniform.
> It appears to me like a mesh. Could someone tell me
> proper contents
> for the silver plating bath with their accurate
> proportions?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing