MEMSnet Home: MEMS-Talk: Adhesion of evaporated Au on Pt layer
Adhesion of evaporated Au on Pt layer
2007-02-21
Rashed Mahameed
2007-02-21
Brent Garber
2007-02-22
Kirt Williams
2007-02-22
WANG,TAK
Adhesion of evaporated Au on Pt layer
WANG,TAK
2007-02-22
Au can go onto platinum without problem.

TK

-----Original Message-----
From: Rashed Mahameed [mailto:[email protected]]
Sent: Wednesday, February 21, 2007 9:07 AM
To: [email protected]
Subject: [mems-talk] Adhesion of evaporated Au on Pt layer

Hi everybody,

Does anybody know if I can evaporate Au directly to Pt without adhesion
layer (e.g. NiCr)? Is there a good adhesion between the two layers?

I need to deposit a couple of microns of Au on Pt.

Thanks,
Rashed
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
MEMS Technology Review