MEMSnet Home: MEMS-Talk: SU-8 on glass
SU-8 on glass
2007-03-16
Yue Mun Pun, Jeffrey
2007-03-16
Gareth Jenkins
SU-8 on glass
Gareth Jenkins
2007-03-16
The thermal conductivity of your wafer has little effect on the SU-8
baking parameters. It will be approximately the same as for silicon.
However, there are other issues relating to coating SU-8 on glass which
have been discussed in depth on this list - have a look at the archives
for more details.

Yue Mun Pun, Jeffrey wrote:
> Hi,
> Has anyone coated and baked SU-8 on borosilicate glass wafers?  Silicon has a
thermal conductivity of 130W/m.K, while borosilicate glass has a thermal
conductivity of 1.4W/m.K.  So for the same baking time on Silicon, glass needs
about 100 times longer baking time on the hot plate.
> Can anyone advise me if I were to coat SU-8 on glass wafers?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Addison Engineering