MEMSnet Home: MEMS-Talk: Pin holes in evaporated Chromium, Titanium and Gold
Pin holes in evaporated Chromium, Titanium and Gold
2007-03-19
Yue Mun Pun, Jeffrey
2007-03-19
Shay Kaplan
2007-03-19
David Casale
2007-03-20
Yue Mun Pun, Jeffrey
Pin holes in evaporated Chromium, Titanium and Gold
David Casale
2007-03-19
Pin holes are pretty common in evaporated chrome. We evap chrome on glass pretty
often, and we often do two coating runs if we want to eliminated pinholes.
Pinholes are much more likely to happen if the chamber and or the substrate is
dirty. For instance, you are much more likely to have pinholes if you evap a
single 1000 angstrom film of chrome than if you do two 500 angstrom coatings.
Cleanliness is next to godliness ;)

Dave Casale
MLA

-----Original Message-----
From: Yue Mun Pun, Jeffrey [mailto:[email protected]]
Sent: Monday, March 19, 2007 2:20 AM
To: General MEMS discussion
Subject: [mems-talk] Pin holes in evaporated Chromium, Titanium and Gold

Hi,
I'm just wondering if anybody has observed pin holes in thermally or e-beam
evaporated Chromium, Titanium and Gold.  If so, how thick do I have to evaporate
these metal films for the pin holes to disappear?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review
Harrick Plasma, Inc.