MEMSnet Home: MEMS-Talk: RE: aluminum bowing
RE: aluminum bowing
1998-06-17
Jason Tauscher
RE: aluminum bowing
Jason Tauscher
1998-06-17
Aluminum is highly stressed and easily attacked.  Either alter the
deposition method/rate/etc. to reduce stress or switch materials.  We make
nickel structures with much success.

--Jason Tauscher
        Silicon Designs, Inc.
        www.silicondesigns.com

-----Original Message-----
From: Robert Dean [mailto:[email protected]]
Sent: Saturday, June 13, 1998 2:32 PM
To: [email protected]
Subject: aluminum bowing


Hello,

I am trying to fabricate a suspended aluminum (99% Al, 0.5% Si, 0.5% Cu)
structure, 1.15um thick on a silicon wafer.  The suspended length is
approximately 130um.  After the structure is released etched from the
silicon using XeF2, the aluminum bridge bows and twists due to stresses.
What causes this and how can I prevent it?  Thank you.

Sincerely,

Robert Dean
RF CMOS Designer
MEMS Optical
205 Import Circle
Suite 2
Huntsville, AL 35806
Tel. 256-859-1886
FAX 256-859-5890
email [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Tanner EDA by Mentor Graphics