Gao Xiaotong
2007-03-23
Pradeep Dixit
glass etching
Pradeep Dixit
2007-03-23
You can check Prof. Eshashi paper in JMEMS. He has shown the pyrex glass
etching by DRIE ..i thik aspect ratio is abt 4. You can also check Ciprian
Illiescu's paper in 'surface and coating' on wet etching of glass.

Thanks,
Pradeep


On 3/22/07, Gao Xiaotong  wrote:
>
> Dear all,
> I plan to etch penetrating holes on glass substrate. But I am worrying
> about the aspect ratio. Could anybody give me some ideas about high aspect
> ration glass etching?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer