MEMSnet Home: MEMS-Talk: Vertical SU-8 walls
Vertical SU-8 walls
2007-03-26
Abhishek Jain
2007-03-30
Gareth Jenkins
2007-03-30
Abhishek Jain
2007-03-31
Gareth Jenkins
2007-04-01
Abhishek Jain
2007-04-03
Nodes Norbert
2007-04-03
Gareth Jenkins
2007-04-03
Abhishek Jain
2007-04-05
Gareth Jenkins
Vertical SU-8 walls
Gareth Jenkins
2007-03-30
What are you using for the exposure?
I would guess either your source isn't well collimated or your mask is
not well contacted with the wafer.

Abhishek Jain wrote:
> I am making SU-8 2025 masters on Si for PDMS replica molding. I use a
> mylar mask and the structures are ~25um tall. I have a problem that I
> do not get good vertical walls of SU-8. A 15um feature comes out as a
> flat length of ~30um and then a linearly decaying thickness that makes
> a total feature size of ~60um.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Harrick Plasma, Inc.