Dear friends,

I am using SU-8 to do the molding. Every time after UV exposure, I get a
broadened pattern than the photomask. 200um wide photomask will probably
result in a 400um wide channel. It's terrible. I doubt that is because the
light source we are using. It's not parallel light. Can anybody recommend
a parallel light source? Or, there is other possible reasons for the
broadened pattern. What are the solutions?
Thanks!

Peng

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group
University Wafer