A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Solvent spin-on PDMS
Solvent spin-on PDMS
2007-03-29
Benedict Samuel
2007-03-30
Joseph Grogan
2007-03-30
Keunho Ahn
2007-03-30
Barbara Cortese
2007-03-30
Heiko van der Linden
Tungsten 'W' etch
2007-03-30
shimul saha
2007-03-30
Anil Agiral
2007-03-31
Andrea Mazzolari
Silicon carbide wet etch
2007-03-30
Andrea Mazzolari
Solvent spin-on PDMS
Keunho Ahn
2007-03-30
for the question 1,
try Hexane, and check PDMS data sheet for other solvents.


On 3/29/07, Benedict Samuel  wrote:
>
> Hi everyone,
> 1. I am trying to get a conformal spin-on coating on top of a flat piece
> of cured PDMS. As long as the coating is transparent and thin (under a few
> microns) I dont care about the solvent/coat used. Any suggestions?
> 2. Can anyone direct me to a process that can make PDMS surface very
> hydrophillic and the effect to last for atleast 30 mins?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation