MEMSnet Home: MEMS-Talk: silicon carbide stiffness tensor
Bonding gold wires to gold electrode
2007-05-11
Yue Mun Pun, Jeffrey
2007-05-11
shay kaplan
2007-05-11
Adamson, Steve
silicon carbide stiffness tensor
2007-05-13
Andrea Mazzolari
2007-05-14
Michael D Martin
silicon carbide stiffness tensor
Andrea Mazzolari
2007-05-13
Hi all, i'm looking for silicon carbide stiffness tensor. Can some one
provide it or suggest me where to find it ?

Best regards,
Andrea Mazzolari