E-beam evaporation of Chrome on uncrosslinked SU-8
2007-05-29
Yue Mun Pun, Jeffrey
2007-05-29
shay kaplan
amount of swelling
2007-05-30
Rajib Ahmed
2007-05-30
Matthew Coda
Diamond
2007-05-31
Andrea Mazzolari
2007-05-31
shay kaplan
2007-05-31
Andrea Mazzolari
2007-06-01
Rick Williston
Diamond
Rick Williston
2007-06-01
Andrea
=20
I can almost guarantee you that you don't need or don't want 2mm thick =
diamond for any real world application. The cost will be prohibitive and =
there are other ways of getting the desired effect of diamond. If you =
just need hardness, or hardness and smoothness then consider =
polycrystalline thick film diamond (I assume you've considered other =
materials almost as hard?). If you need diamond and need it 2mm thick =
for mounting, try a piece 0.5mm thick or less and attach it to =
something, perhaps braze it to a metal backplate and bring your cost =
down. And secondly, if you can bring the 70mm dimension down as well =
your cost gets a lot lower as well.=20
=20
Just do a search for thick film polycrystalline diamond manufacturer and =
you should find someone. If you don't have any luck call me at =
514-938-8089 ext 233 and I'll give you a place to start.
=20
Rick Williston
Microbridge Technologies

>Sorry for the mistake, i'm looking for diamond, not germanium
>Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation