D. Zhou
2007-06-06
Rana, Mukti M
2007-06-07
Raj Gupta
Absorbance measurement of multi-layer structures
D. Zhou
2007-06-01
Dear all,

I am now working on the design and characterisation of multi-layer
structures for efficient mid- or far-infrared radiation absorbers. I not
sure how to measure the absorption of the fabricated structure, for
example, a metal/Si/metal sandwich structure. In our group we can only
conduct transmission measurement. So how can we extract absorbance from the
transmission data? Please give me some hints if you have any experience in
this. Thanks very much.

Cheers,

--
Da-xiang Zhou
PhD candidate
Semiconductor Physics Group
Cavendish Laboratory
University of Cambridge
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
Mentor Graphics Corporation