MEMSnet Home: MEMS-Talk: remove SU8 dry etching
remove SU8 dry etching
2007-06-14
Zhang Xiao Qiang
2007-06-14
[email protected]
remove SU8 dry etching
[email protected]
2007-06-14
Zhang:

It takes a special plasma system to remove SU-8 as you describe. The system
needs to run oxygen and fluorine using a downstream+RIE configuration. Also
cooling of the wafer is important. Under the right process conditions you could
expect 6-10 micron/minute etch rate with no residues. If you want additional
information you can contact me directly. Bob Henderson 480-967-9333


-----Original Message-----
From: Zhang Xiao Qiang 
To: [email protected]
Sent: Wed, 13 Jun 2007 9:29 pm
Subject: [mems-talk] remove SU8 dry etching

Hi, Dear collegues
I would like to remove the  SU8 dry etching after electroplating. The
hickness is about 20 micron. Do you think it is feasible? Anyone like
hare your experience and recipe with me?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing