MEMSnet Home: MEMS-Talk: Drie support wafer
Drie support wafer
2007-06-14
ashwini jambhalikar
2007-06-14
[email protected]
2007-06-14
Jim Beall
2007-06-15
Xiaoguang Liu
2007-06-15
Jim Beall
2007-06-18
Xiaoguang Liu
2007-06-15
Xiaoguang Liu
(211) silicon wafers
2007-06-16
Andrea Mazzolari
Drie support wafer
Jim Beall
2007-06-14
We use a thin layer of Crystalbond 509C wax to bond Si wafers to
backing wafers. You have to watch out for bubbles in the wax or you
can have die pop up.

Jim
On Jun 13, 2007, at 10:39 PM, ashwini jambhalikar wrote:

> Dear Friends,
>
> Can anybody suggest me a better option than cool grease, for
> through etching
> in DRIE .
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review