A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Increasing PDMS bonding to glass without using oxygen plasma
Increasing PDMS bonding to glass without using oxygen plasma
2007-06-19
Virginia Abranches de Sousa R. Soares
2007-06-19
Kevin Christ
Increasing PDMS bonding to glass without using oxygen plasma
Kevin Christ
2007-06-19
You could try using the corona wand method detailed here:

http://www.rsc.org/publishing/journals/LC/article.asp?doi=b610567j

I have found that the bonds it creates are generally not as strong as when using
a standard plasma chamber, but it still works pretty well.

Kevin

-------------------------
Kevin V. Christ
Turner Research Group, http://ktgroup.me.wisc.edu
Department of Mechanical Engineering
University of Wisconsin, Madison
-------------------------

----- Original Message -----
From: "Virginia Abranches de Sousa R. Soares" 
Date: Tuesday, June 19, 2007 10:31 am
Subject: [mems-talk] Increasing PDMS bonding to glass without using oxygen
plasma
To: [email protected]


> Dear Listers,
>
>  Our plasma tool has broken down and we are looking for alternative
> ways of  getting an irreversible bond between PDMS and glass.
>
>  We have searched the web but so far could not find anything that
> would not include an oxygen or an argon plasma.
>
>  Does anybady know if there is some chemical treatment that would
> increase the bonding strength of PDMS?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.