MEMSnet Home: MEMS-Talk: Silicone spin coating of steel membranes
Silicone spin coating of steel membranes
2007-07-02
Markus Herz
Silicone spin coating of steel membranes
Markus Herz
2007-07-02
Hello community,

In a prior project we spin coated steel membranes with silicone, but
adhesion was not satisfying. Metal is not a good adhesion partner for
silicone, roughening or a primer would perhaps help. Any other
recommendations are greatly appreciated!


Best Regards

Markus Herz