About AL protection in TMAH.
2007-07-09
abhaya joshi
About AL protection in TMAH.
abhaya joshi
2007-07-09
Dear All
i am working on Si etching using TMAH. I am looking for AL protection. In
order to achieve it, i am adding Silisic acid (1.4wt%) and Ammonium
persilpahte (0.7wt%) in 5 Wt% TMAH.
With this etchants, In actually experiment, AL layer is getting etched.
Can be one suggest me, how to achieve AL protection in TMAH with acceptable
Si etching rate.
-
Abhay joshi
Universaity of Pune.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.