MEMSnet Home: MEMS-Talk: Any suggestions on through holes on Glass pyrex 7740 wafer
Any suggestions on through holes on Glass pyrex 7740 wafer
2007-07-30
Steven Yang
hybrid integration
2007-07-30
rakesh babu
2007-07-30
[email protected]
Any suggestions on through holes on Glass pyrex 7740 wafer
[email protected]
2007-07-30
How thick is your glass?

Thank you.

John  Bishop
President
Norsam Technologies, Inc.