MEMSnet Home: MEMS-Talk: Bonding PDMS to SU-8
Bonding PDMS to SU-8
2007-09-20
Yue Mun Pun, Jeffrey
Bonding PDMS to SU-8
Yue Mun Pun, Jeffrey
2007-09-20
Hi,
I intend to bond PDMS to SU-8 and the PDMS will be used as a substitute for
glass lid.  Can anyone suggest ways for a reliable bonding technique?

Mr. Jeffrey Mun Pun YUE
余文彬
Division of Bioengineering
E3A-07-02, Nanobioanalytics Lab
7 Engineering Drive 1
National University of Singapore
Singapore 117574
Tel: (65) 65166482, Fax: (65) 68723069
E-mail:  [email protected]
Website:  http://www.bioeng.nus.edu.sg/people/trau/Lab_index.htm
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
The Branford Group