Non-vertical sidewalls of SU8
2007-09-24
Peng Li
Non-vertical sidewalls of SU8
Peng Li
2007-09-24
Dear all,

What could be the reason of non-vertical sidewalls of SU8 mold? I got
pattern with wider bottom and narrower top. The depth of the mold is
400um. The width of the pattern varies from 20um to 80um with space
between them changes from 80um to 20um. I develop the wafer face down for
30mins with gentle shaking. Any comments? Thanks!

Best,

Peng
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation