MEMSnet Home: MEMS-Talk: Haze during wet oxidation
Haze during wet oxidation
2007-10-01
Shivalik Bakshi
2007-10-02
[email protected]
Haze during wet oxidation
Shivalik Bakshi
2007-10-01
Hello,

After undergoing a 1um wet oxidation @ 1050C, I notice a haze pattern on my
silicon wafers. Sometimes there is ring of haze around the wafer edge while the
center is clear. Other times, the center has haze while the edges are clear.

It is only visible under a strong white light.

Has anyone seen this occur on their wafers? Or come across literature that
discuss this?

Thanks a lot,

Shivalik

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
University Wafer