Dear Members,

I am a Ph.D candidate from the City College of New York. I am trying to setup an
electrochemical etching process to manufacture porous silicon using silicon. I
would also like to know the apparatus that are required and their manufacturers.
It would be great if anyone could assit me with this. Thank you.

Kind regards
N Narasimhan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.