MEMSnet Home: MEMS-Talk: Indium Deposition
Indium Deposition
2007-10-23
jpt sharma
2007-10-23
[email protected]
2007-10-23
Bill Moffat
Indium Deposition
jpt sharma
2007-10-23
Hi All
  I am thinking of depositing indium for metal lift off. I am wondering anyone
has done this before? Can we deposit Indium by thermal?

  Thanks
  J. Sharma