MEMSnet Home: MEMS-Talk: nickel deactivation
nickel deactivation
2007-11-07
Rajib Ahmed
nickel deactivation
Rajib Ahmed
2007-11-07
Hello everyone,

We work with Carbon nanotubes grown on copper foils using a nickel
catalyst.  Once the tubes are formed, is there a process to deactivate
or get rid of the nickel caps from the nanotubes without causing any
structural damage to the surface?  Any help would be greatly
appreciated.  Thanks!

--
Rajib Ahmed, Ph.D.
Staff Research Engineer
Bay Materials, LLC./ Cantimer, Inc.
3700 Haven Court
Menlo Park, CA 94025-1043
Phone # (650)474-0500 X 313
Fax # (650)474-0599
Email Address: [email protected]
www.baymaterials.com
www.cantimer.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing