MEMSnet Home: MEMS-Talk: Thin Film problem
Thin Film problem
2007-11-27
Yeswanth Rao
Thin Film problem
Yeswanth Rao
2007-11-27
I have been depositing thin metallic films on glass substrate using an E-beam
evaporator in the following order:

Ti(15nm)/Cu(200nm)/Al(1.2micron) - After deposition, I anodize the aluminum
layer and during anodization at constant potential the current is 2mA - This
process works fine!

But, when I use the following sample: Ti(15nm)/Au(200nm)/Al(1.2micron) and after
e-beam deposition, when I anodize the film at constant potential, the current is
100-140mA which is unusually high. After anodizing for a couple of minutes, the
aluminum lays just dissolves away.

Does anyone have any suggestions as to why this may be happening. Is the problem
associated with the deposition of these metallic layers or something else? Any
information or suggestions will be very helpful

Yeswanth L Rao
UGA
Athens, GA
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation