A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: High Thickness of Aluminum on Silicon
High Thickness of Aluminum on Silicon
2008-01-21
Jacques FATTACCIOLI
2008-01-21
Andrea Mazzolari
2008-01-21
Hong Chen
2008-01-22
Jacques FATTACCIOLI
2008-01-22
shay kaplan
2008-01-22
Gary Hillman
Selective, clean PDMS etch
2008-01-23
Rick Giuly
2008-01-22
David Nemeth
2008-01-21
shay kaplan
High Thickness of Aluminum on Silicon
Andrea Mazzolari
2008-01-21
Yes, this is possible with screen printing. Maybe there are other methods,
i don't know.
At physics department of Ferrara University we have the possibility to
realize such depositions.
Best regards,
Andrea

> Hi All !
>
> For my process, I would like to know if there is an "easy" way to get
> a thick (300microns > t > 30 microns) layer of bare aluminum on a
> silicon wafer ?
> Evaporation and Sputtering are not suitable for this...
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.
University Wafer