MEMSnet Home: MEMS-Talk: Pattern Au electrode on PDMS?
Pattern Au electrode on PDMS?
2008-04-08
Steven Yang
Pattern Au electrode on PDMS?
Steven Yang
2008-04-08
Hi all

I am trying to find a way to pattern Au electrode on PDMS, while keep
the PDMS surface still sticky to be applied later on Si surface as the
cover to seal the microchannel.

I searched and found someone mentioned a Au transfer from Si to PDMS
methode. However, I firstly doubt that the Au can be patterned on Si
with easy transfer property or not? Because the pattern must go
through photoresist removel process which will aslo attack the metal
that not adhered solidly. Secondly, I also doubt the PDMS will stick
on Si without easy to peal off?

So, except this method, is it possible to pattern Au electrode on PDMS
while still keep the PDMS surface sticky enough to make a solid
bonding with silicon substrate? Any suggestion?

Thanks and regards,
Yuming
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group