su8 1000um thick
Abhishek Jain
2008-04-13
Dear forum members

I want to make 1mm thick structures on SU8 for doing soft lithography with
PDMS later on. It is only one mask and just straight channels.

I have SU8 2075 with me and I am trying to find a recipe for doing this. If
anyone has experience in dealing with this, I will truly appreciate if you
may give some insight on the method...

thanks a lot in advance

-Abhishek Jain

--
Research Assistant
Edwin L. Steele Lab for Tumor Biology
149 13th Street
Massachusetts General Hospital
Harvard Medical School
Charlestown MA 02129

Graduate Student
Biomedical Engineering
Boston University
44 Cummington Street
Boston MA 02215

http://steele.mgh.harvard.edu/CV/CV.php?ID=66
http://people.bu.edu/ajain
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review