Hi everybody,

I know that once ITO is sputtered over glass substrate, some companies
offer it with a thin layer of SiO2 for passivation.

Does anyone know if this layer is also sputtered?

Thank you in advance.

Regards,

Rafael García Valverde

Becario de Investigación / Ph.D.student
Departamento de Electrónica, Tecnología de Computadoras
y Proyectos /
Electronics, Computer Tecnology and Projects Department

UNIVERSIDAD POLITÉCNICA DE CARTAGENA.
Campus Muralla del Mar. C/Doctor Fleming s/n, 30202
Cartagena. Spain

email: [email protected]
Tf: 34-968-398787
Fax:0034-968-325400

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing