MEMSnet Home: MEMS-Talk: Etch chemistry for HF wet-etch on Glass
Etch chemistry for HF wet-etch on Glass
2008-04-25
Haixin Zhu
2008-04-25
Roger Shile
Etch chemistry for HF wet-etch on Glass
Haixin Zhu
2008-04-25
Dear all,

We have been trying to understand the chemistry during the HF wet-etch
on borosilicate glass. It turns out the different combination of acid
(HCL, H3PO4) with HF results different etch rate. We believe the
impurity inside the glass caused this change of etch rate. But not sure
the exact chemical reaction happened in this process. Any one have any
suggestions or refer me to some reference papers?

Appreciate the help.

Michael
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
MEMStaff Inc.
Process Variations in Microsystems Manufacturing