MEMSnet Home: MEMS-Talk: Gold evaporation coating on silicon.
Gold evaporation coating on silicon.
2008-05-01
Moshe
2008-05-01
Andrea Mazzolari
2008-05-01
Shay Kaplan
2008-05-01
Roger Shile
2008-05-01
Roger Shile
2008-05-01
Kevin Paul Nichols
Gold evaporation coating on silicon.
Andrea Mazzolari
2008-05-01
Hello,
i whould suggest you to deposit some nm of cr before gold deposition.
Best regards,
Andrea

> Hello
>
> I want to coat silicon with evaporation coating, and
> to assurance that the adhesion between the two
> materials  will be optimal.
> What will be  the optimal treatment to achieve
> adhesion ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
The Branford Group