MEMSnet Home: MEMS-Talk: Wet chemical etch for 316L stainless steel
Wet chemical etch for 316L stainless steel
2008-05-02
Novak Farrington
2008-05-02
Kevin Paul Nichols
2008-05-03
Andrea Mazzolari
2008-05-03
shay kaplan
2008-05-06
Sarosh K
Wet chemical etch for 316L stainless steel
Novak Farrington
2008-05-02
Hi All,

Does anyone know of a wet chemical etch for 316L stainless steel? We're
trying to uniformly etch away, or at least thin, 100um of stainless steel
from a magnesium diboride core. It would be nice if the magnesium diboride
core was not etched, or at least etched at a much slower rate than the
stainless steel.

Thanks in advance,

Novak Farrington
Microelectronics and Nanostructures Group
School of Electrical and Electronic Engineering
Sackville Street Building
The University of Manchester
Manchester M60 1QD


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing