A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Solvent effects on Teflon AF
Teflon Patterning
2008-04-21
Teimour Maleki
2008-04-21
SEBESTA Edward
Solvent effects on Teflon AF
2008-05-09
Teimour Maleki
2008-05-12
Brubaker Chad
2008-04-21
Bill Moffat
2008-04-21
Michael Larsson
Solvent effects on Teflon AF
Brubaker Chad
2008-05-12
Teimour,

Teflon AF should not actually be soluble in IPA. However, depending on
method of use, it may cause mechanical removal (peelng).


Best Regards,
Chad Brubaker

EV Group
invent * innovate * implement
Senior Process Technology Engineer - Direct: +1 (480) 305 2414, Main: +1
(480) 305 2400 Fax: +1 (480) 305 2401
Cell: +1 (602) 321 6071
E-Mail: [email protected], Web: www.EVGroup.com

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Teimour Maleki
Sent: Friday, May 09, 2008 8:07 AM
To: 'General MEMS discussion'
Subject: [mems-talk] Solvent effects on Teflon AF

Dear all,

 Does anybody know what is the effect of IPA on Teflon AF coated
substrate?
When I used IPA, it will remove the Teflon.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group