PDMS glue recommandation
Teimour Maleki
2008-05-28
What do you want to attach together? I used crazy glue from walmart, it
works fine for tubing!!
Have fun,


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Hong Chen
Sent: Wednesday, May 28, 2008 11:37 AM
To: [email protected]
Subject: [mems-talk] PDMS glue recommandation

Hi,

is there anyone can recommend a PDMS glue? I found epoxy-based and
ethylene- vinyl- acetate-based is not useful. Well, you can use PDMS
as the glue but the problem is it trends to spread and occupy every
spaces it can reach including your micro channels.

Hong
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.