pdms removal
2008-06-28
Jose Guevarra
2008-06-28
Mohd.Yusuf
pdms removal
Mohd.Yusuf
2008-06-28
u can use Acetone to clean the dish. i am not sure about wafer...

yusuf

On Sat, Jun 28, 2008 at 4:50 PM, Jose Guevarra  wrote:

> Hi,
>
>  I use a silicon wafer with su-8 as a mold in a petri dishfor PDMS. After
> the PDMS is solidified I remove it by peeling it off.
>
> How do I thoroughly clean off the solidified PDMS from the wafer and petri
> dish?
>

--
Mohd.Yusuf.S.Mulla
Student-FH Jena, Germany.
Currently at :- Leuven, Belgium
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group
University Wafer